DIN 17155 19Mn6 gas cylinders and gas vessels tube forgings forging temperature: heating temperature of 1200 ℃, heat 1 min • mm-1, initial forging temperature 1100 ~ 1150 ℃, the final forging temperature ≥850 ℃, air cooling after forging, heat treatment after forging using positive, the heating temperature is 910 ~ 940 ℃, holding time of 1 min • mm-1 air-cooled .

DIN 17155 19Mn6 gas cylinders and gas vessels tube Chemical composition(%)
Grades
C
max
Si max
Mn.
max
P
max
S
max
N
max
AL
min
Nb max
Ti max
V
max
19Mn6
0.2
0.5
0.7
0.025
0.015
0.009
0.02
0.05
0.03
-
19Mn6 steel pipe Mechanical properties

Grades
Yield Strength
ReH[N/mm2]
transv.min.
 Tensile
Strength
Rm[N/mm2]transv.
Fracture
Elongation
[%]transv. min.

19Mn6



    thickness Total elongation A1
   
  < 3 mm   ≥ 19%
355
510 - 620 ≥ 3 mm ≥ 24%